Sonstiges, Englisch, 484 Seiten, Format (B × H): 125 mm x 142 mm, Gewicht: 200 g
Sonstiges, Englisch, 484 Seiten, Format (B × H): 125 mm x 142 mm, Gewicht: 200 g
ISBN: 978-3-03859-692-9
Verlag: Trans Tech Publications
High performance materials are needed in many thermomechanical applications, such as advanced jet engines or gas turbines, thermal protection of space planes, thermal engineering and nuclear fusion. Ceramic-matrix composites, reinforced with long fibers, are expected to be the most promising candidates for such applications. However, several key problems will have to be solved in the near future. These problems include, above all, the development of a superior thermomechanical performance and oxidation resistance for ceramic fibers and composites, highly efficient protection against corrosion, better fiber/matrix interface design and performance, and cost effective processing.
Autoren/Hrsg.
Weitere Infos & Material
Processing of Ceramic Matrix CompositesDevelopment of SiC Fiber-Reinforced SiC Composites by Radiation-Cured Preceramic PolymerNew Type of Sintered SiC Fiber and Its Composite MaterialFabrication of Carbon Fiber/SiSiC Composites and Their Mechanical PropertiesDispersion of Chopped Short Fibers in Production of Fibers-Reinforced Glass-Ceramic Matrix CompositesSol-Gel Derived Al2O3 Fiber Dispersed with Fine YAG ParticlesChemical and Mechanical Degradation of Hi-Nicalon and Hi-Nicalon-S Fibers under CVD/CVI BN Processing ConditionsStudies of the Spinnability of Polycarbosilane and Spinning Technology of Its Continuous FibersSiC-Based Fibers Synthesized from Hybrid Polymer of Polycarbosilane and PolyvinylsilaneFabrication of Cf/SiC Ceramic Matrix Composites by Polymer Precursor PyrolysisThe Development of a Combustion Chamber Liner Utilizing a Long-Fiber Reinforced Composite Material Made Using the Poly-Silazane Impregnation Method and the Chemical Vapor Deposition MethodDevelopment of Lanthanumhexaluminate Fiber-Coating via Sol-Gel-Route Using Inorganic and Organic PrecursorsDamage Tolerant Oxide Ceramics Using Pure Fiber and Matrix LaminatesHigh Performance Tyranno (Si-C-M-O) Fibers for CompositesMechanical Properties an Microstructural Characteristics of Carbon Fiber Reinforced Silicon Carbide Matrix Composites by Chemical Vapor InfiltrationAn Effective Process for Silicon Carbide Matrix Composites: Dual-Composition Solution Impregnation and Pyrolysis under Medium PressureSol-Gel Processing of Silicon Based Matrixes for Carbon Fiber Reinforced Ceramic CompositesDevelopment and Properties of an Oxide Fiber-Oxide Matrix CompositeProcessing and Microstructure of Polymer-Derived Oxide Composite MaterialsFabrication and Mechanical Properties of Reaction Sintered Silicon Carbide Matrix CompositeSiC Fiber Reinforced Si3N4 Ceramics with Self-Diagnosis FunctionProcessing and Mechanical Properties of C-Fiber Reinforced SiCN-CMCsProcessing and Characterization of Carbon Fiber Reinforced Ceramic NanocompositesIn-situ Synthesis and Oxidation Resistance of C-SiC-TiC-TiB2 CompositeFabrication and Characterization of 3D C/SiC Composites via Slurry and PCVI Joint ProcessProcessing and Characterisation of Silicon Carbide Fibre Reinforced MoSi2-Based CompositesProcess and Properties of Fiber-Reinforced Ceramic Matrix Composites with Function of Fracture DetectionMicromechanical Analysis of CMC Structural Members Based on Homogenization MethodMechanical Properties of Coating Free SiTiCO Fiber-Reinforced SiC Matrix CompositesMechanical Properties of Carbon Fiber-Reinforced hBN Matrix Composites at Elevated TemperatureFracture Behavior of Unidirectional Si-Ti-C-O Fiber- Bonded Ceramic Composite MaterialsMechanical Properties of C/C CompositesGeometry Determination of Cruciform-Type Specimen and Biaxial Tensile Test of C/C CompositesModelling of the Mechanical Behavior of a 2.5D C/C Composite under Tensile and Shear Loads at Room TemperatureDamage Modelling at the Mesoscopic Scale for 4D Carbon/Carbon CompositesFormation of a CVI-SiC Matrix Coating Reinforced by Carbon Fiber on a 2-D Woven C/C SubstrateDetermination of the Interlaminar Tensile Strength of a C/C-Composite by the Diametral Compression Test at Temperatures up to 1800?CShear Failure Behavior of Continuous Fiber Reinforced Ceramic Matrix CompositesAnomalous Strain Behaviour under Stress Controlled Loading of CFCCsToughened Silicon Carbide Based Composites by Microstructure Design and ProcessingA Novel Technique of Using Interfacial Debonding to Measure Fiber-Bridging Stress in Ceramic CompositesThemomechanical Behavior and Microstructure of Tyrannohex CompositesFracture Behavior of Cross-Ply Laminates Carbon-Carbon CompositesCreep Behavior and Modeling of SiC-Based PC Ceramic Matrix Composites with Glass Sealant in High Temperature AirIn situ Properties of 3-D Woven SiC/SiC-Based CompositeProbabilistic-Statistical Approach to Matrix Cracking in Ceramic Matrix Composites (CMCs)Failure Mechanisms and the Macro-Response of Carbon Fiber Reinforced SiC Matrix CompositesTriaxially Braided C/SiC Composites: Research and Development by the Combined Process of CVI+PIPMicrostructure and Mechanical Properties of Hot-Pressed Silicon Carbide Fiber-Reinforced Silicon Carbide CompositeTensile Matrix Cracking Behavior of Hi-Nicalon Fiber/Glass Matrix Cross-Ply Laminate CompositesEffect of the Open Porosity on the Flexural Strength of 2-D Woven Carbon Fiber Reinforced SiC/C Matrix Composites by Reaction-BondingThe Pretreatment on Carbon Fibers for C/SiC CompositesTriaxially Braided C/SiC Composites: Structure and PropertiesTriaxially Braided C/SiC Composites: A High Temperature, Lightweight, Nozzle MaterialThree Dimensional Crack-Fiber Interaction Process in Fiber-Reinforced Ceramic Matrix Composite: Model ExperimentMechanical Behavior of a Si-Ti-C-O Fiber-Bonded Ceramic MaterialStatic Fatigue of 2D SiC/SiC Composites with Multilayered (PyC-SiC)n Interphases at High Temperatures in AirOn the Way to the Equivalence between Measured Parameters Using Non-Notched and Notched Woven Specimens of SiC/C/SiC CompositesDesign of Room Temperature Tensile Test Specimen Made of Ceramic Matrix CompositesFrom the Yarn to the Bulk: A Meso-Macro Approach of the Mechanical Behaviour of 2D Ceramic Matrix CompositesHigh Temperature Behaviours of Two Nanocomposite Oxide FibresThermal Stability of Glass-Sealed Si-Ti-C-O Fiber Reinforced SiC CompositeStructure and Materials of a Multi-Layer Coating for the Oxidation Protection of C/C Composites up to 1700?CThermal Expansion Behaviour of High Melting Point OxidesCharacterization of Coating Cracks in Oxidation-Resistant SiC Coating on C/C CompositesHigh-Temperature Properties of Newly Developed Advanced SiC FibersOxidation Behavior of Glass-Protected Tyranno-Hex Ceramic Matrix CompositesEffects of Matrix Cracking on the Creep of SiC-SiC MicrocompositesTensile Creep Properties of Si-M-C-O (M=Ti or Zr) Fibers in Air Derived from Polymer PrecursorsSome Recommendations for Long Term High Temperature TestsCreep at the Mesoscopic and Microscopic Scale of 2.5D Cf-SiCMacroscopic Creep of 2.5D Cf-SiCFatigue Behavior at High Temperature in Air of a 2D Woven SiC/SiBC with a Self Healing MatrixCyclic Fatigue Behaviour at Room Temperature and at High Temperature under Inert Atmosphere of a C/SiC Multilayer CompositeImprovement of Cyclic Fatigue Analysis by the Use of a Tensile Master Curve in Carbon/Carbon CompositesSubcritical Crack Growth Mechanisms and Failure Mechanism Maps for Ceramic Matrix CompositesNanocreep of Carbon Fibers in 2.5D Cf-SiCTensile Behavior of Woven Ceramic Matrix Composites at Room and Elevated Temperature: An Experimental and Numerical StudyThermal Cycling, Thermal Aging and Thermal Shock Behavior of Nicalon-Fiber Reinforced Glass Matrix CompositesDevelopment of Interfaces in Oxide Matrix Composites(PyC/SiC)n and (BN/SiC)n Nanoscale-Multilayered Interphases by Pressure Pulsed-CVIMultilayerd Interphases in SiC/SiC Composites: Influence of the Interfacial Bond Strength on the Interfacial CharacteristicsA Multilayer Ceramic Matrix for Oxidation Resistant Carbon Fibers-Reinforced CMCsMethodology for Assessing the Interfacial Sliding Stress of a 2D Woven SiC-SiC CompositeModeling of Interfacial Debonding in Unidirectionally Fiber-Reinforced CeramicsRole of Roughness in Fibre/Matrix Interface BehaviourMullite/ZrO2 Laminate Composites for High Temperature ApplicationsFiber Reinforced Porous Alumina Substrate Consisting of Layer with Distinct Grain SizesOxidation Behavior of Ceramic Fibers from the Si-C-N-O System and Sub-SystemsPolyfunctional Interface Coatings for High Temperature Resistant Ceramic Composite of SiC/SiC TypeProperties of Advanced Fibers for SiC/SiC Composite Applications in Fusion Energy SystemsDesigning of Textile Preforms for Ceramic Matrix CompositesDesign, Fabrication and Characterization of High Temperature Joints in Ceramic CompositesDesign of High Preformance CMC Brake DiscsTailoring of Interface Mechanical Properties in Al2O3 Fiber-Reinforced Al2O3 Matrix CompositeMorphology of Ceramic Matrix CompositesJoining of Si-Ti-C-O Fiber Reinforced Ceramic Composite and Fe-Cr-Ni Stainless SteelDevelopment of High Temperature Materials Including CMCs for Space ApplicationCMC for Hot Structures and Control Surfaces of Future LaunchersLow Cost Processing for C/C-SiC Composites by Means of Liquid Silicon Infiltration